| MOQ: | 50 |
| Price: | 12.35 |
| Element | Content (%) | Element | Content (%) |
|---|---|---|---|
| Nickel | 58.0 min. | Silicon | 0.50 |
| Chromium | 20.0-23.0 | Phosphorus | 0.015 |
| Molybdenum | 8.0-10.0 | Sulfur | 0.015 |
| Iron | 5.0 | Aluminum | 0.40 |
| Niobium + Tantalum | 3.15-4.15 | Titanium | 0.40 |
| Carbon | 0.10 | Cobalt | 1.0 |
| Manganese | 0.50 |
| Property | Value |
|---|---|
| Density | 0.305 lbs/in³ (8.44 g/cm³) |
| Specific Heat | 0.102 BTU/lb-°F (427 J/kg-°K) |
| Modulus of Elasticity | 30.1 x 10⁶ psi (207.5 GPa) |
| Thermal Conductivity | 75 BTU/hr/ft²/ft/°F (10.8 W/m-°K) |
| Melting Range | 2350-2460°F (1290-1350°C) |
| Electrical Resistivity | 50.8 Microhm-in at 70°C (128.9 Microhm-cm at 210°C) |
| Yield Strength (0.2% Offset) | Ultimate Tensile Strength | Elongation in 2 in. | Hardness |
|---|---|---|---|
| 65,000 psi (448 MPa) | 125,000 psi (862 MPa) | 50% | 200 Brinell |
| MOQ: | 50 |
| Price: | 12.35 |
| Element | Content (%) | Element | Content (%) |
|---|---|---|---|
| Nickel | 58.0 min. | Silicon | 0.50 |
| Chromium | 20.0-23.0 | Phosphorus | 0.015 |
| Molybdenum | 8.0-10.0 | Sulfur | 0.015 |
| Iron | 5.0 | Aluminum | 0.40 |
| Niobium + Tantalum | 3.15-4.15 | Titanium | 0.40 |
| Carbon | 0.10 | Cobalt | 1.0 |
| Manganese | 0.50 |
| Property | Value |
|---|---|
| Density | 0.305 lbs/in³ (8.44 g/cm³) |
| Specific Heat | 0.102 BTU/lb-°F (427 J/kg-°K) |
| Modulus of Elasticity | 30.1 x 10⁶ psi (207.5 GPa) |
| Thermal Conductivity | 75 BTU/hr/ft²/ft/°F (10.8 W/m-°K) |
| Melting Range | 2350-2460°F (1290-1350°C) |
| Electrical Resistivity | 50.8 Microhm-in at 70°C (128.9 Microhm-cm at 210°C) |
| Yield Strength (0.2% Offset) | Ultimate Tensile Strength | Elongation in 2 in. | Hardness |
|---|---|---|---|
| 65,000 psi (448 MPa) | 125,000 psi (862 MPa) | 50% | 200 Brinell |