logo
Products
PRODUCTS DETAILS
Home > Products >
Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance

Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance

MOQ: 50
Price: 2.35
Detail Information
Certification
AISI
Model NO.:
321 S32168
Shape:
Flat
Technique:
Cold Rolled
Surface Treatment:
Bright
Specification:
1220*2440, 1500*3000, 1500*6000, 2000*6000mm
Thickness:
0.1 To 100 Mm
Width:
10-2500mm
Length:
2m, 2.44m, 3m, Or As Required
Hardness:
Soft, Hard, Half Hard, Quarter Hard, Spring Hard
Carbon Content:
0.08
Chromium Content:
17.0-19.0
Nickel Content:
9.0-12.0
Yield Strength:
30 Ksi
Tensile Strength:
75 Ksi
Elongation:
40%
Highlight:

Titanium Stabilized Stainless Steel Plate

,

High Temperature Resistance 321 Stainless Steel Plate

,

Intergranular Corrosion Resistant S32168 Stainless Steel Plate

Product Description
Stainless Steel 321 / 321H Sheet & Plate Overview
Grade 321 stainless steel is a titanium-stabilized austenitic stainless steel designed for service in the 1000-1600°F temperature range. This grade offers excellent resistance to intergranular corrosion and polythionic acid stress corrosion cracking when given a stabilizing treatment at 1550-1650°F followed by air cooling.
321 stainless steel is readily weldable by all common methods including submerged arc welding. Recommended weld fillers include AWS ER347 bare wire and E347 covered electrodes. With a machinability rating of 45% relative to AISI B1112, it offers similar machining characteristics to 304 stainless steel.
Available Product Forms
Sheet, plate, coil, strip, wire, pipe, tube, bar, profile, round, flat, square, and hexagonal forms.
Specifications & Standards
Specification Details
Primary Standards ASTM A240, ASME SA240, BS EN 10028-7, BS EN 10088-2, BS EN 10088-4
Additional Standards EN 10088/2, EN 10088/4 with CE Marking, NACE MR 0175/ISO 15156 Certification
International Standards ASTM A480, ASTM A959, ASME IID, EN ISO 9445, EN ISO 18286, EN 10051, EN 10088-1, ISO 15510
Dimensions & Tolerances
Parameter Range
Thickness 0.1 to 100 mm
Width 10-2500 mm (600mm-2030 mm typical)
Length 300-6000 mm (Max 18000 mm)
Cold Rolled Plate 0.5-6.4 mm
Hot Rolled Plate 3.0-10.0 mm
Surface Finishes
SATIN, 2B, 2D, BA NO (8), Cold rolled sheet (CR), Hot rolled plate (HR), No.1 finish hot rolled, 1D, No.4, BA, 8K, hairline, brush, mirror, etching, SB, Ti-coating, color-coating, embossing.
Hardness Options
Soft, Hard, Half Hard, Quarter Hard, Spring Hard
Trade Names & Designations
SS 321, SUS 321, Inox 321, DIN 1.4541, UNS S32100, AISI 321, SAE 321 Sheet
Applications
  • Aircraft piston engine manifolds
  • Expansion joints
  • Firearms production
  • Thermal oxidizers
  • Refinery equipment
  • High temperature chemical process equipment
Chemical Composition
Element Content (%)
Carbon 0.08 max
Chromium 17.0-19.0
Nickel 9.0-12.0
Manganese 2.00 max
Silicon 0.75 max
Nitrogen 0.10 max
Phosphorus 0.045 max
Sulfur 0.030 max
Titanium 5(C+N) min / 0.70 max
Mechanical Properties
Property Value
Yield Strength, min. 30 ksi
Tensile Strength, min. 75 ksi
Elongation, min. 40%
Hardness, max. 95 Rb
Physical Properties
Property Value
Density 0.286 lb/in³
Modulus of Elasticity 28.0 x 10⁶ psi
Coefficient of Thermal Expansion (68-212°F) 9.2 x 10⁻⁶ /°F
Thermal Conductivity 9.3 Btu/ft hr °F
Specific Heat 0.12 Btu/lb °F
Electrical Resistivity 28.4 Microohm-in
International Grade Equivalents
Standard Designation
UNS S32100
EN/Euronorm 1.4541, X6CrNiTi18-10
JIS SUS 321
BS 321S31
GOST 08X18H10T, 06Ch18N10T, 12X18H10T
GB 0Cr18Ni11Ti
DIN 1.4541, 1.4544
AFNOR Z6CNT18-10, Z10CNT18-11
Alternative Grades Comparison
Alternative Grade Application Consideration
304L When resistance to intergranular corrosion is required without high-temperature strength needs
3CR12 For mild high-temperature environments up to approximately 600°C
304H For mild high-temperature environments up to approximately 800°C
310 For operating environments up to approximately 1100°C
S30815 (253MA) For operating environments up to approximately 1150°C
Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance 0 Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance 1 Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance 2 Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance 3 Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance 4 Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance 5
Products
PRODUCTS DETAILS
Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance
MOQ: 50
Price: 2.35
Detail Information
Certification
AISI
Model NO.:
321 S32168
Shape:
Flat
Technique:
Cold Rolled
Surface Treatment:
Bright
Specification:
1220*2440, 1500*3000, 1500*6000, 2000*6000mm
Thickness:
0.1 To 100 Mm
Width:
10-2500mm
Length:
2m, 2.44m, 3m, Or As Required
Hardness:
Soft, Hard, Half Hard, Quarter Hard, Spring Hard
Carbon Content:
0.08
Chromium Content:
17.0-19.0
Nickel Content:
9.0-12.0
Yield Strength:
30 Ksi
Tensile Strength:
75 Ksi
Elongation:
40%
Minimum Order Quantity:
50
Price:
2.35
Highlight

Titanium Stabilized Stainless Steel Plate

,

High Temperature Resistance 321 Stainless Steel Plate

,

Intergranular Corrosion Resistant S32168 Stainless Steel Plate

Product Description
Stainless Steel 321 / 321H Sheet & Plate Overview
Grade 321 stainless steel is a titanium-stabilized austenitic stainless steel designed for service in the 1000-1600°F temperature range. This grade offers excellent resistance to intergranular corrosion and polythionic acid stress corrosion cracking when given a stabilizing treatment at 1550-1650°F followed by air cooling.
321 stainless steel is readily weldable by all common methods including submerged arc welding. Recommended weld fillers include AWS ER347 bare wire and E347 covered electrodes. With a machinability rating of 45% relative to AISI B1112, it offers similar machining characteristics to 304 stainless steel.
Available Product Forms
Sheet, plate, coil, strip, wire, pipe, tube, bar, profile, round, flat, square, and hexagonal forms.
Specifications & Standards
Specification Details
Primary Standards ASTM A240, ASME SA240, BS EN 10028-7, BS EN 10088-2, BS EN 10088-4
Additional Standards EN 10088/2, EN 10088/4 with CE Marking, NACE MR 0175/ISO 15156 Certification
International Standards ASTM A480, ASTM A959, ASME IID, EN ISO 9445, EN ISO 18286, EN 10051, EN 10088-1, ISO 15510
Dimensions & Tolerances
Parameter Range
Thickness 0.1 to 100 mm
Width 10-2500 mm (600mm-2030 mm typical)
Length 300-6000 mm (Max 18000 mm)
Cold Rolled Plate 0.5-6.4 mm
Hot Rolled Plate 3.0-10.0 mm
Surface Finishes
SATIN, 2B, 2D, BA NO (8), Cold rolled sheet (CR), Hot rolled plate (HR), No.1 finish hot rolled, 1D, No.4, BA, 8K, hairline, brush, mirror, etching, SB, Ti-coating, color-coating, embossing.
Hardness Options
Soft, Hard, Half Hard, Quarter Hard, Spring Hard
Trade Names & Designations
SS 321, SUS 321, Inox 321, DIN 1.4541, UNS S32100, AISI 321, SAE 321 Sheet
Applications
  • Aircraft piston engine manifolds
  • Expansion joints
  • Firearms production
  • Thermal oxidizers
  • Refinery equipment
  • High temperature chemical process equipment
Chemical Composition
Element Content (%)
Carbon 0.08 max
Chromium 17.0-19.0
Nickel 9.0-12.0
Manganese 2.00 max
Silicon 0.75 max
Nitrogen 0.10 max
Phosphorus 0.045 max
Sulfur 0.030 max
Titanium 5(C+N) min / 0.70 max
Mechanical Properties
Property Value
Yield Strength, min. 30 ksi
Tensile Strength, min. 75 ksi
Elongation, min. 40%
Hardness, max. 95 Rb
Physical Properties
Property Value
Density 0.286 lb/in³
Modulus of Elasticity 28.0 x 10⁶ psi
Coefficient of Thermal Expansion (68-212°F) 9.2 x 10⁻⁶ /°F
Thermal Conductivity 9.3 Btu/ft hr °F
Specific Heat 0.12 Btu/lb °F
Electrical Resistivity 28.4 Microohm-in
International Grade Equivalents
Standard Designation
UNS S32100
EN/Euronorm 1.4541, X6CrNiTi18-10
JIS SUS 321
BS 321S31
GOST 08X18H10T, 06Ch18N10T, 12X18H10T
GB 0Cr18Ni11Ti
DIN 1.4541, 1.4544
AFNOR Z6CNT18-10, Z10CNT18-11
Alternative Grades Comparison
Alternative Grade Application Consideration
304L When resistance to intergranular corrosion is required without high-temperature strength needs
3CR12 For mild high-temperature environments up to approximately 600°C
304H For mild high-temperature environments up to approximately 800°C
310 For operating environments up to approximately 1100°C
S30815 (253MA) For operating environments up to approximately 1150°C
Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance 0 Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance 1 Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance 2 Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance 3 Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance 4 Titanium Stabilized 321 Stainless Steel Plate with High Temperature Resistance and Intergranular Corrosion Resistance 5