logo
Products
PRODUCTS DETAILS
Home > Products >
Super Duplex S32750 2507 Stainless Steel Plate with High Strength and Chloride Stress Corrosion Cracking Resistance

Super Duplex S32750 2507 Stainless Steel Plate with High Strength and Chloride Stress Corrosion Cracking Resistance

MOQ: 50
Price: 6.55
Detail Information
Certification
ISO, AISI
Model NO.:
S25073 S32750 DIN1.4410 2507
Shape:
Round
Technique:
Hot Rolled
Surface Treatment:
Pickling
Specification:
1220*2440, 1500*3000, 1500*6000, 2000*6000mm
Chromium Content:
25%
Molybdenum Content:
4%
Nickel Content:
7%
Nitrogen Content:
0.27%
Yield Strength:
80 Ksi Min
Tensile Strength:
116 Ksi Min
Elongation:
15% Min
Hardness:
32 Rockwell C Max
Impact Energy:
74 Ft.-lbs. Min
PREN Value:
≥ 40
Highlight:

Corrosion Resistant Super Duplex Stainless Steel Plate

,

High Strength S32750 Stainless Steel Plate

,

Chloride Stress Corrosion Cracking Resistance 2507 Stainless Steel Plate

Product Description
Super Duplex S25073 S32750 DIN1.4410 2507 Stainless Steel Plate
Alloy 2507 (UNS S32750) is a super duplex stainless steel with 25% chromium, 4% molybdenum, and 7% nickel designed for demanding applications requiring exceptional strength and corrosion resistance. This steel offers excellent resistance to chloride stress corrosion cracking, high thermal conductivity, and low coefficient of thermal expansion. The high chromium, molybdenum, and nitrogen levels provide superior resistance to pitting, crevice, and general corrosion.
Standards & Specifications
ASTM/ASME: A240 - UNS S32750
EURONORM: 1.4410 - X2 Cr Ni MoN 25.7.4
AFNOR: Z3 CN 25.06 Az
Industrial Applications
  • Oil and gas industry equipment
  • Offshore platforms, heat exchangers, and process water systems
  • Chemical process industries, vessels, and piping
  • Desalination plants and seawater piping systems
  • Mechanical and structural components requiring high strength
  • Power industry FGD systems and scrubber systems
Chemical Composition
Typical values (Weight %)
C Cr Ni Mo N Others
0.020 25 7 4.0 0.27 S=0.001
PREN Formula: [Cr%] + 3.3 [Mo%] + 16 [N%] ≥ 40
Mechanical Properties
Property Value
0.2% Offset Yield Strength, ksi 80 min.
Ultimate Tensile Strength, ksi 116 min.
0.1% Offset Yield Strength, ksi 91 min.
Elongation in 2 inches, % 15 min.
Hardness Rockwell C 32 max.
Impact Energy, ft.-lbs. 74 min.
Temperature Limitation: Not recommended for applications requiring long exposures above 570°F due to potential reduction in toughness.
Product Gallery
Products
PRODUCTS DETAILS
Super Duplex S32750 2507 Stainless Steel Plate with High Strength and Chloride Stress Corrosion Cracking Resistance
MOQ: 50
Price: 6.55
Detail Information
Certification
ISO, AISI
Model NO.:
S25073 S32750 DIN1.4410 2507
Shape:
Round
Technique:
Hot Rolled
Surface Treatment:
Pickling
Specification:
1220*2440, 1500*3000, 1500*6000, 2000*6000mm
Chromium Content:
25%
Molybdenum Content:
4%
Nickel Content:
7%
Nitrogen Content:
0.27%
Yield Strength:
80 Ksi Min
Tensile Strength:
116 Ksi Min
Elongation:
15% Min
Hardness:
32 Rockwell C Max
Impact Energy:
74 Ft.-lbs. Min
PREN Value:
≥ 40
Minimum Order Quantity:
50
Price:
6.55
Highlight

Corrosion Resistant Super Duplex Stainless Steel Plate

,

High Strength S32750 Stainless Steel Plate

,

Chloride Stress Corrosion Cracking Resistance 2507 Stainless Steel Plate

Product Description
Super Duplex S25073 S32750 DIN1.4410 2507 Stainless Steel Plate
Alloy 2507 (UNS S32750) is a super duplex stainless steel with 25% chromium, 4% molybdenum, and 7% nickel designed for demanding applications requiring exceptional strength and corrosion resistance. This steel offers excellent resistance to chloride stress corrosion cracking, high thermal conductivity, and low coefficient of thermal expansion. The high chromium, molybdenum, and nitrogen levels provide superior resistance to pitting, crevice, and general corrosion.
Standards & Specifications
ASTM/ASME: A240 - UNS S32750
EURONORM: 1.4410 - X2 Cr Ni MoN 25.7.4
AFNOR: Z3 CN 25.06 Az
Industrial Applications
  • Oil and gas industry equipment
  • Offshore platforms, heat exchangers, and process water systems
  • Chemical process industries, vessels, and piping
  • Desalination plants and seawater piping systems
  • Mechanical and structural components requiring high strength
  • Power industry FGD systems and scrubber systems
Chemical Composition
Typical values (Weight %)
C Cr Ni Mo N Others
0.020 25 7 4.0 0.27 S=0.001
PREN Formula: [Cr%] + 3.3 [Mo%] + 16 [N%] ≥ 40
Mechanical Properties
Property Value
0.2% Offset Yield Strength, ksi 80 min.
Ultimate Tensile Strength, ksi 116 min.
0.1% Offset Yield Strength, ksi 91 min.
Elongation in 2 inches, % 15 min.
Hardness Rockwell C 32 max.
Impact Energy, ft.-lbs. 74 min.
Temperature Limitation: Not recommended for applications requiring long exposures above 570°F due to potential reduction in toughness.