| MOQ: | 100 |
| Price: | 2.15 |
| Element (%) | 304 | 304L | 304H |
|---|---|---|---|
| Carbon (C) | 0.0 - 0.07 | 0.0 - 0.03 | 0.04 - 0.08 |
| Manganese (Mn) | 0.0 - 2.0 | 0.0 - 2.00 | 0.0 - 2.0 |
| Silicon (Si) | 0.0 - 1.00 | 0.0 - 1.00 | 0.0 - 1.0 |
| Phosphorus (P) | 0.0 - 0.05 | 0.0 - 0.05 | 0.0 - 0.04 |
| Sulfur (S) | 0.0 - 0.03 | 0.0 - 0.02 | 0.0 - 0.02 |
| Chromium (Cr) | 17.50 - 19.50 | 17.50 - 19.50 | 17.00 - 19.00 |
| Nickel (Ni) | 8.00 - 10.50 | 8.00 - 10.50 | 8.00 - 11.00 |
| Nitrogen (N) | 0.0 - 0.11 | 0.0 - 0.11 | 0.0 - 0.10 |
| Iron (Fe) | Balance | ||
| Property | 304 | 304L |
|---|---|---|
| Tensile Strength (MPa) | 520 - 720 | 500 - 700 |
| Proof Stress (MPa) | 210 Min | 200 Min |
| Elongation A5 | 45 Min % | 45 Min % |
| Property | 304 | 304L | 304H |
|---|---|---|---|
| Tensile Strength (MPa) | 500 - 700 | 500 - 700 | 500 - 700 |
| Proof Stress (MPa) | 190 | 175 Min | 185 Min |
| Elongation A50 mm | 45 Min % | 45 Min % | 40 Min % |
| Hardness Brinell | 215 Max HB | 215 Max HB | - |
| Property | Value |
|---|---|
| Density | 8.00 g/cm³ |
| Melting Point | 1450 °C |
| Modulus of Elasticity | 193 GPa |
| Electrical Resistivity | 0.72 x 10⁻⁶ Ω.m |
| Thermal Conductivity | 16.2 W/m.K |
| Thermal Expansion | 17.2 x 10⁻⁶/K |
| Minimum Order Quantity | 1 Ton |
| Price Term | FOB |
| Payment | L/C at sight or 30% TT as deposit |
| Delivery Time | 20-30 days after receiving deposit |
| Samples | Free samples with express charges borne by customer |
| MOQ: | 100 |
| Price: | 2.15 |
| Element (%) | 304 | 304L | 304H |
|---|---|---|---|
| Carbon (C) | 0.0 - 0.07 | 0.0 - 0.03 | 0.04 - 0.08 |
| Manganese (Mn) | 0.0 - 2.0 | 0.0 - 2.00 | 0.0 - 2.0 |
| Silicon (Si) | 0.0 - 1.00 | 0.0 - 1.00 | 0.0 - 1.0 |
| Phosphorus (P) | 0.0 - 0.05 | 0.0 - 0.05 | 0.0 - 0.04 |
| Sulfur (S) | 0.0 - 0.03 | 0.0 - 0.02 | 0.0 - 0.02 |
| Chromium (Cr) | 17.50 - 19.50 | 17.50 - 19.50 | 17.00 - 19.00 |
| Nickel (Ni) | 8.00 - 10.50 | 8.00 - 10.50 | 8.00 - 11.00 |
| Nitrogen (N) | 0.0 - 0.11 | 0.0 - 0.11 | 0.0 - 0.10 |
| Iron (Fe) | Balance | ||
| Property | 304 | 304L |
|---|---|---|
| Tensile Strength (MPa) | 520 - 720 | 500 - 700 |
| Proof Stress (MPa) | 210 Min | 200 Min |
| Elongation A5 | 45 Min % | 45 Min % |
| Property | 304 | 304L | 304H |
|---|---|---|---|
| Tensile Strength (MPa) | 500 - 700 | 500 - 700 | 500 - 700 |
| Proof Stress (MPa) | 190 | 175 Min | 185 Min |
| Elongation A50 mm | 45 Min % | 45 Min % | 40 Min % |
| Hardness Brinell | 215 Max HB | 215 Max HB | - |
| Property | Value |
|---|---|
| Density | 8.00 g/cm³ |
| Melting Point | 1450 °C |
| Modulus of Elasticity | 193 GPa |
| Electrical Resistivity | 0.72 x 10⁻⁶ Ω.m |
| Thermal Conductivity | 16.2 W/m.K |
| Thermal Expansion | 17.2 x 10⁻⁶/K |
| Minimum Order Quantity | 1 Ton |
| Price Term | FOB |
| Payment | L/C at sight or 30% TT as deposit |
| Delivery Time | 20-30 days after receiving deposit |
| Samples | Free samples with express charges borne by customer |