| MOQ: | 50 |
| Price: | 3.15 |
| Electrical resistivity (µOhm.cm) | 70-73 |
| Elongation at break (%) | <60 |
| Hardness - Brinell | 160-190 |
| Izod impact strength (J.m⁻¹) | 20-136 |
| Modulus of elasticity (GPa) | 190-210 |
| Tensile strength (MPa) | 520-1100 |
| Density (g.cm⁻³) | 7.93 |
| Melting point (°C) | 1400-1425 |
| Coefficient of thermal expansion (x10⁻⁶ K⁻¹) | 16-18 @ 20-100°C |
| Maximum use temperature in air (°C) | 800 |
| Thermal conductivity | 16.4 W/mK | 114 BTU in/hr.ft².°F |
| Thermal expansion co-efficient (@0.000-100°C/32-212°F) | 11 µm/m°C | 6.11 µin/in°F |
| MOQ: | 50 |
| Price: | 3.15 |
| Electrical resistivity (µOhm.cm) | 70-73 |
| Elongation at break (%) | <60 |
| Hardness - Brinell | 160-190 |
| Izod impact strength (J.m⁻¹) | 20-136 |
| Modulus of elasticity (GPa) | 190-210 |
| Tensile strength (MPa) | 520-1100 |
| Density (g.cm⁻³) | 7.93 |
| Melting point (°C) | 1400-1425 |
| Coefficient of thermal expansion (x10⁻⁶ K⁻¹) | 16-18 @ 20-100°C |
| Maximum use temperature in air (°C) | 800 |
| Thermal conductivity | 16.4 W/mK | 114 BTU in/hr.ft².°F |
| Thermal expansion co-efficient (@0.000-100°C/32-212°F) | 11 µm/m°C | 6.11 µin/in°F |