| MOQ: | 100 |
| Price: | 3.65 |
| ASTM | JIS | AISI | EN |
|---|---|---|---|
| Grade S30100 | SUS301 | 301 | 1.431 |
| S30400 | SUS304 | 304 | 1.4301 |
| S30403 | - | 304L | 1.4307 |
| S31008 | SUS310S | 310S | 1.4845 |
| S31603 | - | 316L | 1.4404 |
| S32100 | SUS321 | 321 | 1.4541 |
| S41008 | SUS410S | 410S | - |
| S43000 | SUS430 | 430 | 1.4016 |
| S43932 | - | - | 1.451 |
| S44400 | SUS444 | 444 | 1.4521 |
| S44500 | SUS430J1L | - | - |
| ASTM Specifications | Additional Standards |
|---|---|
| ASTM A182 Grade FXM-19 ASTM A193 Grade B8R Class 1C ASTM A193 Grade B8R Class 1D ASTM A193 Grade B8RA Class 1C ASTM A194 Grade 8R ASTM A194 Grade 8RA ASTM A213 Grade XM-19 ASTM A240 Grade S20910 ASTM A249 Grade TPXM-19 ASTM A269 Grade TPXM-19 ASTM A276 Grade S20910 ASTM A312 Grade TPXM-19 ASTM A314 Grade S20910 ASTM A336 Grade FXM-19 ASTM A358 Grade A240 XM-19 ASTM A403 Grade CRXM-19 ASTM A403 Grade WPXM-19 ASTM A479 Grade S20910 ASTM A580 Grade S20910 ASTM A813 Grade TPXM-19 ASTM A814 Grade TPXM-19 ASTM A943 Grade TPXM-19 ASTM A959 Grade S20910 ASTM A965 Grade FXM-19 |
AISI XM-19 SAE XM-19 UNS S20910 |
| Element | Min (%) | Max (%) |
|---|---|---|
| C | 0.05 | 0.10 |
| Mn | - | 0.80 |
| Si | 1.10 | 2.00 |
| P | - | 0.040 |
| S | - | 0.030 |
| Cr | 20.0 | 22.0 |
| Ni | 10.0 | 12.0 |
| N | 0.14 | 0.20 |
| Ce | 0.03 | 0.08 |
| Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness Rockwell B (HR B) max | Hardness Brinell (HB) max |
|---|---|---|---|---|
| 600 | 310 | 40 | 95 | 217 |
| Property | Value |
|---|---|
| Density (kg/m³) | 7800 |
| Elastic Modulus (GPa) | 200 |
| Mean Coefficient of Thermal Expansion 0-100°C (mm/m/°C) | 17.0 |
| Mean Coefficient of Thermal Expansion 0-600°C (mm/m/°C) | 18.5 |
| Mean Coefficient of Thermal Expansion 0-1000°C (mm/m/°C) | 19.5 |
| Thermal Conductivity at 20°C (W/m.K) | 15.0 |
| Thermal Conductivity at 1000°C (W/m.K) | 29.0 |
| Specific Heat 0-100°C (J/kg.K) | 500 |
| Electrical Resistivity (nW.m) | 850 |
| UNS No | Euronorm | Swedish SS | Japanese JIS |
|---|---|---|---|
| S30815 | 1.4835 X9CrNiSiNCe21-11-2 | 2368 | - |
| Grade | Selection Criteria |
|---|---|
| 310 | Carburising atmospheres require a higher nickel content |
| 304H | Lower cost alternative, provided the operating temperature is below about 800°C |
| Nickel Alloys | Carburising atmospheres or temperatures above the 1100-1150°C maximum of 253MA |
| MOQ: | 100 |
| Price: | 3.65 |
| ASTM | JIS | AISI | EN |
|---|---|---|---|
| Grade S30100 | SUS301 | 301 | 1.431 |
| S30400 | SUS304 | 304 | 1.4301 |
| S30403 | - | 304L | 1.4307 |
| S31008 | SUS310S | 310S | 1.4845 |
| S31603 | - | 316L | 1.4404 |
| S32100 | SUS321 | 321 | 1.4541 |
| S41008 | SUS410S | 410S | - |
| S43000 | SUS430 | 430 | 1.4016 |
| S43932 | - | - | 1.451 |
| S44400 | SUS444 | 444 | 1.4521 |
| S44500 | SUS430J1L | - | - |
| ASTM Specifications | Additional Standards |
|---|---|
| ASTM A182 Grade FXM-19 ASTM A193 Grade B8R Class 1C ASTM A193 Grade B8R Class 1D ASTM A193 Grade B8RA Class 1C ASTM A194 Grade 8R ASTM A194 Grade 8RA ASTM A213 Grade XM-19 ASTM A240 Grade S20910 ASTM A249 Grade TPXM-19 ASTM A269 Grade TPXM-19 ASTM A276 Grade S20910 ASTM A312 Grade TPXM-19 ASTM A314 Grade S20910 ASTM A336 Grade FXM-19 ASTM A358 Grade A240 XM-19 ASTM A403 Grade CRXM-19 ASTM A403 Grade WPXM-19 ASTM A479 Grade S20910 ASTM A580 Grade S20910 ASTM A813 Grade TPXM-19 ASTM A814 Grade TPXM-19 ASTM A943 Grade TPXM-19 ASTM A959 Grade S20910 ASTM A965 Grade FXM-19 |
AISI XM-19 SAE XM-19 UNS S20910 |
| Element | Min (%) | Max (%) |
|---|---|---|
| C | 0.05 | 0.10 |
| Mn | - | 0.80 |
| Si | 1.10 | 2.00 |
| P | - | 0.040 |
| S | - | 0.030 |
| Cr | 20.0 | 22.0 |
| Ni | 10.0 | 12.0 |
| N | 0.14 | 0.20 |
| Ce | 0.03 | 0.08 |
| Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness Rockwell B (HR B) max | Hardness Brinell (HB) max |
|---|---|---|---|---|
| 600 | 310 | 40 | 95 | 217 |
| Property | Value |
|---|---|
| Density (kg/m³) | 7800 |
| Elastic Modulus (GPa) | 200 |
| Mean Coefficient of Thermal Expansion 0-100°C (mm/m/°C) | 17.0 |
| Mean Coefficient of Thermal Expansion 0-600°C (mm/m/°C) | 18.5 |
| Mean Coefficient of Thermal Expansion 0-1000°C (mm/m/°C) | 19.5 |
| Thermal Conductivity at 20°C (W/m.K) | 15.0 |
| Thermal Conductivity at 1000°C (W/m.K) | 29.0 |
| Specific Heat 0-100°C (J/kg.K) | 500 |
| Electrical Resistivity (nW.m) | 850 |
| UNS No | Euronorm | Swedish SS | Japanese JIS |
|---|---|---|---|
| S30815 | 1.4835 X9CrNiSiNCe21-11-2 | 2368 | - |
| Grade | Selection Criteria |
|---|---|
| 310 | Carburising atmospheres require a higher nickel content |
| 304H | Lower cost alternative, provided the operating temperature is below about 800°C |
| Nickel Alloys | Carburising atmospheres or temperatures above the 1100-1150°C maximum of 253MA |