| Cuota De Producción: | 100 |
| Precio: | 3.65 |
| ASTM | JIS | AISI | EN |
|---|---|---|---|
| Grado S30100 | SUS301 | 301 | 1.431 |
| S30400 | SUS304 | 304 | 1.4301 |
| S30403 | - | 304L | 1.4307 |
| S31008 | SUS310S | 310S | 1.4845 |
| S31603 | - | 316L | 1.4404 |
| S32100 | SUS321 | 321 | 1.4541 |
| S41008 | SUS410S | 410S | - |
| S43000 | SUS430 | 430 | 1.4016 |
| S43932 | - | - | 1.451 |
| S44400 | SUS444 | 444 | 1.4521 |
| S44500 | SUS430J1L | - | - |
| Especificaciones ASTM | Normas adicionales |
|---|---|
| ASTM A182 Grado FXM-19 ASTM A193 Grado B8R Clase 1C ASTM A193 Grado B8R Clase 1D ASTM A193 Grado B8RA Clase 1C ASTM A194 Grado 8R ASTM A194 Grado 8RA ASTM A213 Grado XM-19 ASTM A240 Grado S20910 ASTM A249 Grado TPXM-19 ASTM A269 Grado TPXM-19 ASTM A276 Grado S20910 ASTM A312 Grado TPXM-19 ASTM A314 Grado S20910 ASTM A336 Grado FXM-19 ASTM A358 Grado A240 XM-19 ASTM A403 Grado CRXM-19 ASTM A403 Grado WPXM-19 ASTM A479 Grado S20910 ASTM A580 Grado S20910 ASTM A813 Grado TPXM-19 ASTM A814 Grado TPXM-19 ASTM A943 Grado TPXM-19 ASTM A959 Grado S20910 ASTM A965 Grado FXM-19 |
AISI XM-19 SAE XM-19 UNS S20910 |
| Elemento | Mín (%) | Máx (%) |
|---|---|---|
| C | 0.05 | 0.10 |
| Mn | - | 0.80 |
| Si | 1.10 | 2.00 |
| P | - | 0.040 |
| S | - | 0.030 |
| Cr | 20.0 | 22.0 |
| Ni | 10.0 | 12.0 |
| N | 0.14 | 0.20 |
| Ce | 0.03 | 0.08 |
| Resistencia a la tracción (MPa) mín. | Límite elástico 0.2% (MPa) mín. | Alargamiento (% en 50 mm) mín. | Dureza Rockwell B (HR B) máx. | Dureza Brinell (HB) máx. |
|---|---|---|---|---|
| 600 | 310 | 40 | 95 | 217 |
| Propiedad | Valor |
|---|---|
| Densidad (kg/m³) | 7800 |
| Módulo de elasticidad (GPa) | 200 |
| Coeficiente medio de expansión térmica 0-100°C (mm/m/°C) | 17.0 |
| Coeficiente medio de expansión térmica 0-600°C (mm/m/°C) | 18.5 |
| Coeficiente medio de expansión térmica 0-1000°C (mm/m/°C) | 19.5 |
| Conductividad térmica a 20°C (W/m.K) | 15.0 |
| Conductividad térmica a 1000°C (W/m.K) | 29.0 |
| Calor específico 0-100°C (J/kg.K) | 500 |
| Resistividad eléctrica (nW.m) | 850 |
| Nº UNS | Euronorm | Sueco SS | Japonés JIS |
|---|---|---|---|
| S30815 | 1.4835 X9CrNiSiNCe21-11-2 | 2368 | - |
| Grado | Criterios de selección |
|---|---|
| 310 | Las atmósferas de cementación requieren un mayor contenido de níquel |
| 304H | Alternativa de menor costo, siempre que la temperatura de operación esté por debajo de aproximadamente 800°C |
| Aleaciones de níquel | Atmósferas de cementación o temperaturas superiores al máximo de 1100-1150°C del 253MA |
| Cuota De Producción: | 100 |
| Precio: | 3.65 |
| ASTM | JIS | AISI | EN |
|---|---|---|---|
| Grado S30100 | SUS301 | 301 | 1.431 |
| S30400 | SUS304 | 304 | 1.4301 |
| S30403 | - | 304L | 1.4307 |
| S31008 | SUS310S | 310S | 1.4845 |
| S31603 | - | 316L | 1.4404 |
| S32100 | SUS321 | 321 | 1.4541 |
| S41008 | SUS410S | 410S | - |
| S43000 | SUS430 | 430 | 1.4016 |
| S43932 | - | - | 1.451 |
| S44400 | SUS444 | 444 | 1.4521 |
| S44500 | SUS430J1L | - | - |
| Especificaciones ASTM | Normas adicionales |
|---|---|
| ASTM A182 Grado FXM-19 ASTM A193 Grado B8R Clase 1C ASTM A193 Grado B8R Clase 1D ASTM A193 Grado B8RA Clase 1C ASTM A194 Grado 8R ASTM A194 Grado 8RA ASTM A213 Grado XM-19 ASTM A240 Grado S20910 ASTM A249 Grado TPXM-19 ASTM A269 Grado TPXM-19 ASTM A276 Grado S20910 ASTM A312 Grado TPXM-19 ASTM A314 Grado S20910 ASTM A336 Grado FXM-19 ASTM A358 Grado A240 XM-19 ASTM A403 Grado CRXM-19 ASTM A403 Grado WPXM-19 ASTM A479 Grado S20910 ASTM A580 Grado S20910 ASTM A813 Grado TPXM-19 ASTM A814 Grado TPXM-19 ASTM A943 Grado TPXM-19 ASTM A959 Grado S20910 ASTM A965 Grado FXM-19 |
AISI XM-19 SAE XM-19 UNS S20910 |
| Elemento | Mín (%) | Máx (%) |
|---|---|---|
| C | 0.05 | 0.10 |
| Mn | - | 0.80 |
| Si | 1.10 | 2.00 |
| P | - | 0.040 |
| S | - | 0.030 |
| Cr | 20.0 | 22.0 |
| Ni | 10.0 | 12.0 |
| N | 0.14 | 0.20 |
| Ce | 0.03 | 0.08 |
| Resistencia a la tracción (MPa) mín. | Límite elástico 0.2% (MPa) mín. | Alargamiento (% en 50 mm) mín. | Dureza Rockwell B (HR B) máx. | Dureza Brinell (HB) máx. |
|---|---|---|---|---|
| 600 | 310 | 40 | 95 | 217 |
| Propiedad | Valor |
|---|---|
| Densidad (kg/m³) | 7800 |
| Módulo de elasticidad (GPa) | 200 |
| Coeficiente medio de expansión térmica 0-100°C (mm/m/°C) | 17.0 |
| Coeficiente medio de expansión térmica 0-600°C (mm/m/°C) | 18.5 |
| Coeficiente medio de expansión térmica 0-1000°C (mm/m/°C) | 19.5 |
| Conductividad térmica a 20°C (W/m.K) | 15.0 |
| Conductividad térmica a 1000°C (W/m.K) | 29.0 |
| Calor específico 0-100°C (J/kg.K) | 500 |
| Resistividad eléctrica (nW.m) | 850 |
| Nº UNS | Euronorm | Sueco SS | Japonés JIS |
|---|---|---|---|
| S30815 | 1.4835 X9CrNiSiNCe21-11-2 | 2368 | - |
| Grado | Criterios de selección |
|---|---|
| 310 | Las atmósferas de cementación requieren un mayor contenido de níquel |
| 304H | Alternativa de menor costo, siempre que la temperatura de operación esté por debajo de aproximadamente 800°C |
| Aleaciones de níquel | Atmósferas de cementación o temperaturas superiores al máximo de 1100-1150°C del 253MA |