Alloy C22 is an improved nickel-base alloy designed for use in aggressive industrial environments. This alloy offers excellent resistance to pitting and crevice corrosion in oxidizing and acid chloride environments, and is practically immune to chloride stress corrosion cracking (SCC).
| Element | Ni | Cr | Mo | Mn | Si | C | S | P | Cu | V | W | Fe |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| MIN | -- | 20.0 | 12.5 | -- | -- | -- | -- | -- | -- | -- | 2.5 | -- |
| MAX | balance | 22.5 | 14.5 | 0.5 | 0.08 | 0.015 | 0.02 | 0.02 | 2.5 | 0.35 | 3.5 | 6.0 |
| Temperature (°F) | 70 | 200 | 400 | 600 | 800 | 1000 | 1200 | 1400 |
|---|---|---|---|---|---|---|---|---|
| Ultimate Tensile Strength (ksi) | 114 | 107 | 98 | 95 | 92 | 88 | 83 | 76 |
| 0.2% Yield Strength (ksi) | 54 | 49 | 41 | 36 | 35 | 34 | 32 | 31 |
| Elongation (%) | 62 | 65 | 66 | 68 | 68 | 67 | 69 | 68 |
| Hardness MAX (HRB) | 95 | -- | -- | -- | -- | -- | -- | -- |
| Product Form | Standard |
|---|---|
| Pipe Seamless | B622 |
| Pipe Welded | B619 |
| Tube Seamless | B622 |
| Tube Welded | B626 |
| Sheet/Plate | B575 |
| Bar | B574 |
| Forging | B564 |
| Fitting | B366 |
Although ductile enough for cold working, intermediate annealing may be necessary due to work hardening. Forging should be performed between 1750-2050°F followed by rapid cooling. Annealing can be performed at 2020-2150°F followed by rapid quench to avoid formation of detrimental phases. Welding can be done by gas tungsten-arc, gas metal-arc and shielded metal-arc processes.
Alloy C22 is an improved nickel-base alloy designed for use in aggressive industrial environments. This alloy offers excellent resistance to pitting and crevice corrosion in oxidizing and acid chloride environments, and is practically immune to chloride stress corrosion cracking (SCC).
| Element | Ni | Cr | Mo | Mn | Si | C | S | P | Cu | V | W | Fe |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| MIN | -- | 20.0 | 12.5 | -- | -- | -- | -- | -- | -- | -- | 2.5 | -- |
| MAX | balance | 22.5 | 14.5 | 0.5 | 0.08 | 0.015 | 0.02 | 0.02 | 2.5 | 0.35 | 3.5 | 6.0 |
| Temperature (°F) | 70 | 200 | 400 | 600 | 800 | 1000 | 1200 | 1400 |
|---|---|---|---|---|---|---|---|---|
| Ultimate Tensile Strength (ksi) | 114 | 107 | 98 | 95 | 92 | 88 | 83 | 76 |
| 0.2% Yield Strength (ksi) | 54 | 49 | 41 | 36 | 35 | 34 | 32 | 31 |
| Elongation (%) | 62 | 65 | 66 | 68 | 68 | 67 | 69 | 68 |
| Hardness MAX (HRB) | 95 | -- | -- | -- | -- | -- | -- | -- |
| Product Form | Standard |
|---|---|
| Pipe Seamless | B622 |
| Pipe Welded | B619 |
| Tube Seamless | B622 |
| Tube Welded | B626 |
| Sheet/Plate | B575 |
| Bar | B574 |
| Forging | B564 |
| Fitting | B366 |
Although ductile enough for cold working, intermediate annealing may be necessary due to work hardening. Forging should be performed between 1750-2050°F followed by rapid cooling. Annealing can be performed at 2020-2150°F followed by rapid quench to avoid formation of detrimental phases. Welding can be done by gas tungsten-arc, gas metal-arc and shielded metal-arc processes.