| Element | Ni | Cr | Mn | C | Mo | Si | Fe |
|---|---|---|---|---|---|---|---|
| Max | Bal. | 22.5 | 0.50 | 0.015 | 14.5 | 0.08 | 6.0 |
| Min | 20.0 | 12.5 | 2.0 |
| Property | Ultimate Tensile | Yield Strength (0.2% OS) | Elong. in 2 in. (50.8mm) or 4D min., % | R/A | Hardness |
|---|---|---|---|---|---|
| Min | 100 KSi | 45 KSi | 45 | ||
| Max | |||||
| Min | 690 MPa | 310 MPa | |||
| Max |
| Product Form | Specification |
|---|---|
| Bar | ASTM B574 |
| Sheet | ASTM B575 |
| Plate | ASTM B575 |
| Fitting | ASME SB-366 |
| Forging | ASME SB-564 |
| Weld Wire | AWS A5.14 |
| Alloy | Characteristics |
|---|---|
| Hastelloy B-3 alloy | Same excellent resistance to hydrochloric acid and other strongly reducing chemicals as B-2 alloy, but with significantly better thermal stability, fabricability and stress corrosion cracking resistance. |
| Hastelloy HYBRID-BC1 alloy | A new Ni-Cr-Mo alloy with superior resistance to hydrochloric and sulfuric acids, without the drawbacks of the Ni-Mo and Zr materials. Its resistance to these key chemicals is much greater than that of the popular Ni-Cr-Mo (C-type) alloys. |
| Hastelloy C-4 alloy | High-temperature stability in the 1200-1900°F (650-1040°C) range as evidenced by good ductility and corrosion resistance. Virtually the same corrosion resistance as alloy C-276. |
| Hastelloy C-22 alloy | Better overall corrosion resistance in oxidizing corrosives than C-4, C-276 and 625 alloys. Outstanding resistance to localized corrosion and excellent resistance to stress corrosion cracking. |
| Hastelloy C-22HS alloy | This alloy was designed to exhibit corrosion resistance comparable to other C-type alloys, but which can be heat treated to obtain approximately double the yield strength. |
| Hastelloy C-276 alloy | Versatile, corrosion resistant alloy. Very good resistance to reducing, and mildly oxidizing corrosives. Excellent stress corrosion cracking resistance with very good resistance to localized attack. |
| Hastelloy C-2000 alloy | Most versatile, corrosion resistant alloy with excellent resistance to uniform corrosion in oxidizing or reducing environments. Excellent resistance to stress corrosion cracking. |
| Hastelloy G-30 alloy | Many advantages over other metallic and non-metallic materials in handling phosphoric acid, sulfuric acid, nitric acid, fluoride environments and oxidizing acid mixtures. |
| Hastelloy G-35 alloy | Excellent resistance to corrosion in highly oxidizing media and acidic chloride environments. |
| Hastelloy N alloy | Good resistance to aging and embrittlement and good fabricability. It has excellent resistance to hot fluoride salts in the temperature range of 1300°F to 1600°F (705°C-870°C). |
| MOQ: | 50 |
| Price: | 30 |
| Element | Ni | Cr | Mn | C | Mo | Si | Fe |
|---|---|---|---|---|---|---|---|
| Max | Bal. | 22.5 | 0.50 | 0.015 | 14.5 | 0.08 | 6.0 |
| Min | 20.0 | 12.5 | 2.0 |
| Property | Ultimate Tensile | Yield Strength (0.2% OS) | Elong. in 2 in. (50.8mm) or 4D min., % | R/A | Hardness |
|---|---|---|---|---|---|
| Min | 100 KSi | 45 KSi | 45 | ||
| Max | |||||
| Min | 690 MPa | 310 MPa | |||
| Max |
| Product Form | Specification |
|---|---|
| Bar | ASTM B574 |
| Sheet | ASTM B575 |
| Plate | ASTM B575 |
| Fitting | ASME SB-366 |
| Forging | ASME SB-564 |
| Weld Wire | AWS A5.14 |
| Alloy | Characteristics |
|---|---|
| Hastelloy B-3 alloy | Same excellent resistance to hydrochloric acid and other strongly reducing chemicals as B-2 alloy, but with significantly better thermal stability, fabricability and stress corrosion cracking resistance. |
| Hastelloy HYBRID-BC1 alloy | A new Ni-Cr-Mo alloy with superior resistance to hydrochloric and sulfuric acids, without the drawbacks of the Ni-Mo and Zr materials. Its resistance to these key chemicals is much greater than that of the popular Ni-Cr-Mo (C-type) alloys. |
| Hastelloy C-4 alloy | High-temperature stability in the 1200-1900°F (650-1040°C) range as evidenced by good ductility and corrosion resistance. Virtually the same corrosion resistance as alloy C-276. |
| Hastelloy C-22 alloy | Better overall corrosion resistance in oxidizing corrosives than C-4, C-276 and 625 alloys. Outstanding resistance to localized corrosion and excellent resistance to stress corrosion cracking. |
| Hastelloy C-22HS alloy | This alloy was designed to exhibit corrosion resistance comparable to other C-type alloys, but which can be heat treated to obtain approximately double the yield strength. |
| Hastelloy C-276 alloy | Versatile, corrosion resistant alloy. Very good resistance to reducing, and mildly oxidizing corrosives. Excellent stress corrosion cracking resistance with very good resistance to localized attack. |
| Hastelloy C-2000 alloy | Most versatile, corrosion resistant alloy with excellent resistance to uniform corrosion in oxidizing or reducing environments. Excellent resistance to stress corrosion cracking. |
| Hastelloy G-30 alloy | Many advantages over other metallic and non-metallic materials in handling phosphoric acid, sulfuric acid, nitric acid, fluoride environments and oxidizing acid mixtures. |
| Hastelloy G-35 alloy | Excellent resistance to corrosion in highly oxidizing media and acidic chloride environments. |
| Hastelloy N alloy | Good resistance to aging and embrittlement and good fabricability. It has excellent resistance to hot fluoride salts in the temperature range of 1300°F to 1600°F (705°C-870°C). |