| MOQ: | 50 |
| Prijs: | 1.35 |
| Element | Percent by Weight |
|---|---|
| Carbon (C) | 0.15 max |
| Manganese (Mn) | 1.00 max |
| Silicon (Si) | 1.00 max |
| Chromium (Cr) | 11.50 - 13.50 |
| Nickel (Ni) | 0.75 max |
| Sulfur (S) | 0.03 max |
| Phosphorus (P) | 0.04 max |
| Temperature Range | Coefficients |
|---|---|
| 20-200°C (68-392°F) | 10.5 x 10⁻⁶ cm/cm/°C (5.9 x 10⁻⁶ in/in/°F) |
| 20-600°C (68-1112°F) | 11.6 x 10⁻⁶ cm/cm/°C (6.5 x 10⁻⁶ in/in/°F) |
| Temperature | W/m·K | Btu/(hr · ft · °F) |
|---|---|---|
| 100°C (212°F) | 0.249 | 14.4 |
| Temperature | microhm-cm |
|---|---|
| 20°C (68°F) | 56 |
| Typical Annealed Properties | Hardening Response HRC |
|---|---|
| HRB: 82-96 0.2% Offset Yield Strength: 30-42 Ksi (205-290 MPa) Tensile Strength: 65-74 Ksi (450-510 MPa) Elongation: 20-34% in 2" (51 mm) | 38-45 |
| MOQ: | 50 |
| Prijs: | 1.35 |
| Element | Percent by Weight |
|---|---|
| Carbon (C) | 0.15 max |
| Manganese (Mn) | 1.00 max |
| Silicon (Si) | 1.00 max |
| Chromium (Cr) | 11.50 - 13.50 |
| Nickel (Ni) | 0.75 max |
| Sulfur (S) | 0.03 max |
| Phosphorus (P) | 0.04 max |
| Temperature Range | Coefficients |
|---|---|
| 20-200°C (68-392°F) | 10.5 x 10⁻⁶ cm/cm/°C (5.9 x 10⁻⁶ in/in/°F) |
| 20-600°C (68-1112°F) | 11.6 x 10⁻⁶ cm/cm/°C (6.5 x 10⁻⁶ in/in/°F) |
| Temperature | W/m·K | Btu/(hr · ft · °F) |
|---|---|---|
| 100°C (212°F) | 0.249 | 14.4 |
| Temperature | microhm-cm |
|---|---|
| 20°C (68°F) | 56 |
| Typical Annealed Properties | Hardening Response HRC |
|---|---|
| HRB: 82-96 0.2% Offset Yield Strength: 30-42 Ksi (205-290 MPa) Tensile Strength: 65-74 Ksi (450-510 MPa) Elongation: 20-34% in 2" (51 mm) | 38-45 |