| MOQ: | 100 |
| Preis: | 4.65 |
| ASTM | JIS | AISI | Die |
|---|---|---|---|
| Klasse S30100 | SUS301 | 301 | 1.431 |
| S30400 | SUS304 | 304 | 1.4301 |
| S30403 | - | 304L | 1.4307 |
| S31008 | SUS310S | 310S | 1.4845 |
| S31603 | - | 316L | 1.4404 |
| S32100 | SUS321 | 321 | 1.4541 |
| S41008 | SUS410S | 410S | - |
| S43000 | SUS430 | 430 | 1.4016 |
| S43932 | - | - | 1.451 |
| S44400 | SUS444 | 444 | 1.4521 |
| S44500 | SUS430J1L | - | - |
| ASTM A182-Klasse FXM-19 | ASTM A269 Klasse TPXM-19 | ASTM A580 Klasse S20910 |
|---|---|---|
| ASTM A193 Klasse B8R Klasse 1C | ASTM A276 Klasse S20910 | ASTM A813-Klasse TPXM-19 |
| ASTM A193 Klasse B8R Klasse 1D | ASTM A312 Klasse TPXM-19 | ASTM A814-Klasse TPXM-19 |
| ASTM A193 Klasse B8RA Klasse 1C | ASTM A314 Klasse S20910 | ASTM A943 Klasse TPXM-19 |
| ASTM A194 Klasse 8R | ASTM A336 Klasse FXM-19 | ASTM A959 Klasse S20910 |
| ASTM A194 Klasse 8RA | ASTM A358 Klasse A240 XM-19 | ASTM A965-Klasse FXM-19 |
| ASTM A213 Klasse XM-19 | ASTM A403 Klasse CRXM-19 | AISI XM-19 |
| ASTM A240 Klasse S20910 | ASTM A403-Klasse WPXM-19 | SAE XM-19 |
| ASTM A249-Klasse TPXM-19 | ASTM A479 Klasse S20910 | UNS S20910 |
| Elemente | Min (%) | Maximal (%) |
|---|---|---|
| C | 0.05 | 0.10 |
| In | - | 0.80 |
| - Ja. | 1.10 | 2.00 |
| P | - | 0.040 |
| S | - | 0.030 |
| Die | 20.0 | 22.0 |
| Ni | 10.0 | 12.0 |
| N | 0.14 | 0.20 |
| Die | 0.03 | 0.08 |
| Zugfestigkeit (MPa) min | Leistungsfestigkeit 0,2% Proof (MPa) min | Verlängerung (% in 50 mm) min | Rockwell B (HR B) max. | Brinell (HB) max. |
|---|---|---|---|---|
| 600 | 310 | 40 | 95 | 217 |
| Eigentum | Wert |
|---|---|
| Dichte (kg/m3) | 7800 |
| Elastizitätsmodul (GPa) | 200 |
| Durchschnittlicher Wärmeexpansionskoeffizient (mm/m/°C) 0-100°C | 17.0 |
| Durchschnittlicher Koeffizient der thermischen Ausdehnung (mm/m/°C) 0-600°C | 18.5 |
| Durchschnittlicher thermischer Expansionskoeffizient (mm/m/°C) 0-1000°C | 19.5 |
| Wärmeleitfähigkeit (W/m.K) bei 20 °C | 15.0 |
| Wärmeleitfähigkeit (W/m.K) bei 1000°C | 29.0 |
| Spezifische Wärme 0-100°C (J/kg.K) | 500 |
| Elektrische Widerstandsfähigkeit (nW.m) | 850 |
| UNS Nr. | Euronorm Nr. | Euronorm-Name | Schwedische SS | Japanische JIS |
|---|---|---|---|---|
| S30815 | 1.4835 | X9CrNiSiNCe21-11-2 | 2368 | - |
| Zulassung | Warum sollte er statt 253MA gewählt werden? |
|---|---|
| 310 | Vergasungsatmosphären erfordern einen höheren Nickelgehalt |
| 304H | Kostengünstigere Alternative, vorausgesetzt, dass die Betriebstemperatur unter ca. 800°C liegt |
| Nickellegierungen | Vergasungsatmosphären oder Temperaturen über 1100 - 1150 °C maximal 253 MA |
| MOQ: | 100 |
| Preis: | 4.65 |
| ASTM | JIS | AISI | Die |
|---|---|---|---|
| Klasse S30100 | SUS301 | 301 | 1.431 |
| S30400 | SUS304 | 304 | 1.4301 |
| S30403 | - | 304L | 1.4307 |
| S31008 | SUS310S | 310S | 1.4845 |
| S31603 | - | 316L | 1.4404 |
| S32100 | SUS321 | 321 | 1.4541 |
| S41008 | SUS410S | 410S | - |
| S43000 | SUS430 | 430 | 1.4016 |
| S43932 | - | - | 1.451 |
| S44400 | SUS444 | 444 | 1.4521 |
| S44500 | SUS430J1L | - | - |
| ASTM A182-Klasse FXM-19 | ASTM A269 Klasse TPXM-19 | ASTM A580 Klasse S20910 |
|---|---|---|
| ASTM A193 Klasse B8R Klasse 1C | ASTM A276 Klasse S20910 | ASTM A813-Klasse TPXM-19 |
| ASTM A193 Klasse B8R Klasse 1D | ASTM A312 Klasse TPXM-19 | ASTM A814-Klasse TPXM-19 |
| ASTM A193 Klasse B8RA Klasse 1C | ASTM A314 Klasse S20910 | ASTM A943 Klasse TPXM-19 |
| ASTM A194 Klasse 8R | ASTM A336 Klasse FXM-19 | ASTM A959 Klasse S20910 |
| ASTM A194 Klasse 8RA | ASTM A358 Klasse A240 XM-19 | ASTM A965-Klasse FXM-19 |
| ASTM A213 Klasse XM-19 | ASTM A403 Klasse CRXM-19 | AISI XM-19 |
| ASTM A240 Klasse S20910 | ASTM A403-Klasse WPXM-19 | SAE XM-19 |
| ASTM A249-Klasse TPXM-19 | ASTM A479 Klasse S20910 | UNS S20910 |
| Elemente | Min (%) | Maximal (%) |
|---|---|---|
| C | 0.05 | 0.10 |
| In | - | 0.80 |
| - Ja. | 1.10 | 2.00 |
| P | - | 0.040 |
| S | - | 0.030 |
| Die | 20.0 | 22.0 |
| Ni | 10.0 | 12.0 |
| N | 0.14 | 0.20 |
| Die | 0.03 | 0.08 |
| Zugfestigkeit (MPa) min | Leistungsfestigkeit 0,2% Proof (MPa) min | Verlängerung (% in 50 mm) min | Rockwell B (HR B) max. | Brinell (HB) max. |
|---|---|---|---|---|
| 600 | 310 | 40 | 95 | 217 |
| Eigentum | Wert |
|---|---|
| Dichte (kg/m3) | 7800 |
| Elastizitätsmodul (GPa) | 200 |
| Durchschnittlicher Wärmeexpansionskoeffizient (mm/m/°C) 0-100°C | 17.0 |
| Durchschnittlicher Koeffizient der thermischen Ausdehnung (mm/m/°C) 0-600°C | 18.5 |
| Durchschnittlicher thermischer Expansionskoeffizient (mm/m/°C) 0-1000°C | 19.5 |
| Wärmeleitfähigkeit (W/m.K) bei 20 °C | 15.0 |
| Wärmeleitfähigkeit (W/m.K) bei 1000°C | 29.0 |
| Spezifische Wärme 0-100°C (J/kg.K) | 500 |
| Elektrische Widerstandsfähigkeit (nW.m) | 850 |
| UNS Nr. | Euronorm Nr. | Euronorm-Name | Schwedische SS | Japanische JIS |
|---|---|---|---|---|
| S30815 | 1.4835 | X9CrNiSiNCe21-11-2 | 2368 | - |
| Zulassung | Warum sollte er statt 253MA gewählt werden? |
|---|---|
| 310 | Vergasungsatmosphären erfordern einen höheren Nickelgehalt |
| 304H | Kostengünstigere Alternative, vorausgesetzt, dass die Betriebstemperatur unter ca. 800°C liegt |
| Nickellegierungen | Vergasungsatmosphären oder Temperaturen über 1100 - 1150 °C maximal 253 MA |