| MOQ: | 50 |
| Prijs: | 13.5 |
| UNS | Handelsmerk | JIS | W.Nr. |
|---|---|---|---|
| N06600 | Inconel 600 | NCF600 | 2.4816 |
| Elementen | Min (%) | Maximaal (%) |
|---|---|---|
| Ni | 72 | - |
| Cr | 14 | 17 |
| Fe | 6 | 10 |
| C | - | 0.15 |
| Deeltjes | - | 1 |
| - Jawel. | - | 0.5 |
| C. | - | 0.5 |
| P | - | 0.015 |
| S | - | 0.015 |
| Vastgoed | Waarde |
|---|---|
| Dichtheid | 8.4 g/cm3 |
| Smeltepunt | 1370-1425 °C |
| Status van de legering | Tensile sterkte (N/mm2) | Vermogen (N/mm2) | Verlenging A5 (%) | Brinellhardheid (HB) |
|---|---|---|---|---|
| Ontdooiing | 550 | 240 | 30 | 95 |
| Oplossingsbehandeling | 500 | 180 | 35 | 85 |
| MOQ: | 50 |
| Prijs: | 13.5 |
| UNS | Handelsmerk | JIS | W.Nr. |
|---|---|---|---|
| N06600 | Inconel 600 | NCF600 | 2.4816 |
| Elementen | Min (%) | Maximaal (%) |
|---|---|---|
| Ni | 72 | - |
| Cr | 14 | 17 |
| Fe | 6 | 10 |
| C | - | 0.15 |
| Deeltjes | - | 1 |
| - Jawel. | - | 0.5 |
| C. | - | 0.5 |
| P | - | 0.015 |
| S | - | 0.015 |
| Vastgoed | Waarde |
|---|---|
| Dichtheid | 8.4 g/cm3 |
| Smeltepunt | 1370-1425 °C |
| Status van de legering | Tensile sterkte (N/mm2) | Vermogen (N/mm2) | Verlenging A5 (%) | Brinellhardheid (HB) |
|---|---|---|---|---|
| Ontdooiing | 550 | 240 | 30 | 95 |
| Oplossingsbehandeling | 500 | 180 | 35 | 85 |