| MOQ: | 50 |
| Prijs: | 13.5 |
| UNS | Handelsmerk | JIS | W.Nr |
|---|---|---|---|
| N06600 | Inconel600 | NCF600 | 2.4816 |
| Legering | Element | Ni | Cr | Fe | C | Mn | Si | Cu | P | S |
|---|---|---|---|---|---|---|---|---|---|---|
| 600 | Min. | 72 | 14 | 6 | - | - | - | - | - | - |
| Max. | - | 17 | 10 | 0.15 | 1 | 0.5 | 0.5 | 0.015 | 0.015 |
| Dichtheid | Smeltpunt |
|---|---|
| 8,4 g/cm³ | 1370-1425 °C |
| Legering status | Treksterkte Rm N/mm² | Vloeigrens RP0.2 N/mm² | Rek A5 % | Brinell hardheid HB |
|---|---|---|---|---|
| Gloeibehandeling | 550 | 240 | 30 | 95 |
| Oplossingsbehandeling | 500 | 180 | 35 | 85 |
| MOQ: | 50 |
| Prijs: | 13.5 |
| UNS | Handelsmerk | JIS | W.Nr |
|---|---|---|---|
| N06600 | Inconel600 | NCF600 | 2.4816 |
| Legering | Element | Ni | Cr | Fe | C | Mn | Si | Cu | P | S |
|---|---|---|---|---|---|---|---|---|---|---|
| 600 | Min. | 72 | 14 | 6 | - | - | - | - | - | - |
| Max. | - | 17 | 10 | 0.15 | 1 | 0.5 | 0.5 | 0.015 | 0.015 |
| Dichtheid | Smeltpunt |
|---|---|
| 8,4 g/cm³ | 1370-1425 °C |
| Legering status | Treksterkte Rm N/mm² | Vloeigrens RP0.2 N/mm² | Rek A5 % | Brinell hardheid HB |
|---|---|---|---|---|
| Gloeibehandeling | 550 | 240 | 30 | 95 |
| Oplossingsbehandeling | 500 | 180 | 35 | 85 |