| MOQ: | 50 |
| Price: | 3.13 |
| Product | 17-4PH Stainless Steel Round Bar |
|---|---|
| Diameter Range | 8-450mm |
| Length | 6m per piece or custom cutting available |
| Finishing | Black Bar / Bright Bar |
| Available Grades | 201, 301, 303Cu, 304, 304L, 309S, 310S, 316L, 316Ti, 317L, 318, 321, 347, 410, 420, 430, 431, 440a/b/c, 904L, 2205, 2507, Hastelloy C276/C4/C22, Inconel 600/625, Incoloy 800/825/825H |
| Services | Cutting, surface polishing, heat treatment |
| Brands | Walsin, BAOSTEEL, TISCO, QINGSHAN |
| Applications | Standards |
|---|---|
|
|
| Element | Content (%) |
|---|---|
| Carbon (C) | ≤ 0.07 |
| Manganese (Mn) | ≤ 1.00 |
| Silicon (Si) | ≤ 1.00 |
| Phosphorus (P) | ≤ 0.04 |
| Sulfur (S) | ≤ 0.030 |
| Chromium (Cr) | 15.0 - 17.5 |
| Nickel (Ni) | 3.0 - 5.0 |
| Copper (Cu) | 3.0 - 5.0 |
| Niobium + Tantalum (Nb+Ta) | 0.15 - 0.45 |
| Condition | Tensile Strength (MPa) | Yield Strength 0.2% Proof (MPa) | Elongation (% in 50mm) | Hardness Rockwell C |
|---|---|---|---|---|
| Solution Treated | 1105 (typical) | 1000 (typical) | 15 (typical) | 38 max |
| Condition 900 | 1310 min | 1170 min | 10 min | 40 min |
| Condition 1150 | 930 min | 724 min | 16 min | 28 min |
| Property | Value |
|---|---|
| Density | 7750 kg/m³ |
| Thermal Conductivity at 100°C | 18.4 W/m·K |
| Thermal Conductivity at 500°C | 22.7 W/m·K |
| Specific Heat (0-100°C) | 460 J/kg·K |
| Electrical Resistivity | 800 nΩ·m |
| MOQ: | 50 |
| Price: | 3.13 |
| Product | 17-4PH Stainless Steel Round Bar |
|---|---|
| Diameter Range | 8-450mm |
| Length | 6m per piece or custom cutting available |
| Finishing | Black Bar / Bright Bar |
| Available Grades | 201, 301, 303Cu, 304, 304L, 309S, 310S, 316L, 316Ti, 317L, 318, 321, 347, 410, 420, 430, 431, 440a/b/c, 904L, 2205, 2507, Hastelloy C276/C4/C22, Inconel 600/625, Incoloy 800/825/825H |
| Services | Cutting, surface polishing, heat treatment |
| Brands | Walsin, BAOSTEEL, TISCO, QINGSHAN |
| Applications | Standards |
|---|---|
|
|
| Element | Content (%) |
|---|---|
| Carbon (C) | ≤ 0.07 |
| Manganese (Mn) | ≤ 1.00 |
| Silicon (Si) | ≤ 1.00 |
| Phosphorus (P) | ≤ 0.04 |
| Sulfur (S) | ≤ 0.030 |
| Chromium (Cr) | 15.0 - 17.5 |
| Nickel (Ni) | 3.0 - 5.0 |
| Copper (Cu) | 3.0 - 5.0 |
| Niobium + Tantalum (Nb+Ta) | 0.15 - 0.45 |
| Condition | Tensile Strength (MPa) | Yield Strength 0.2% Proof (MPa) | Elongation (% in 50mm) | Hardness Rockwell C |
|---|---|---|---|---|
| Solution Treated | 1105 (typical) | 1000 (typical) | 15 (typical) | 38 max |
| Condition 900 | 1310 min | 1170 min | 10 min | 40 min |
| Condition 1150 | 930 min | 724 min | 16 min | 28 min |
| Property | Value |
|---|---|
| Density | 7750 kg/m³ |
| Thermal Conductivity at 100°C | 18.4 W/m·K |
| Thermal Conductivity at 500°C | 22.7 W/m·K |
| Specific Heat (0-100°C) | 460 J/kg·K |
| Electrical Resistivity | 800 nΩ·m |