| MOQ: | 50 |
| Price: | 3.17 |
| Element | Content (%) |
|---|---|
| C | ≤ 0.07 |
| Mn | ≤ 1.0 |
| Si | ≤ 1.0 |
| P | ≤ 0.04 |
| S | ≤ 0.030 |
| Cr | 15.0 - 17.5 |
| Ni | 3.0 - 5.0 |
| Cu | 3.0 - 5.0 |
| Nb+Ta | 0.15 - 0.45 |
| Condition | Tensile Strength (MPa) | Yield Strength (MPa) | Elongation (%) | Hardness (HRC) |
|---|---|---|---|---|
| Solution Treated | 1105 (typ) | 1000 (typ) | 15 (typ) | 38 max |
| Condition 900 | 1310 min | 1170 min | 10 min | 40 min |
| Condition 1150 | 930 min | 724 min | 16 min | 28 min |
| Property | Value |
|---|---|
| Density | 7750 kg/m³ |
| Thermal Expansion (0-100°C) | 10.8 µm/m/°C |
| Thermal Conductivity (100°C) | 18.4 W/m·K |
| Specific Heat | 460 J/kg·K |
| Electrical Resistivity | 800 nΩ·m |
| MOQ: | 50 |
| Price: | 3.17 |
| Element | Content (%) |
|---|---|
| C | ≤ 0.07 |
| Mn | ≤ 1.0 |
| Si | ≤ 1.0 |
| P | ≤ 0.04 |
| S | ≤ 0.030 |
| Cr | 15.0 - 17.5 |
| Ni | 3.0 - 5.0 |
| Cu | 3.0 - 5.0 |
| Nb+Ta | 0.15 - 0.45 |
| Condition | Tensile Strength (MPa) | Yield Strength (MPa) | Elongation (%) | Hardness (HRC) |
|---|---|---|---|---|
| Solution Treated | 1105 (typ) | 1000 (typ) | 15 (typ) | 38 max |
| Condition 900 | 1310 min | 1170 min | 10 min | 40 min |
| Condition 1150 | 930 min | 724 min | 16 min | 28 min |
| Property | Value |
|---|---|
| Density | 7750 kg/m³ |
| Thermal Expansion (0-100°C) | 10.8 µm/m/°C |
| Thermal Conductivity (100°C) | 18.4 W/m·K |
| Specific Heat | 460 J/kg·K |
| Electrical Resistivity | 800 nΩ·m |