| Applications | Standards |
|---|---|
|
|
| Element | Content (%) |
|---|---|
| C | 0.07 max |
| Mn | 1.0 max |
| Si | 1.0 max |
| P | 0.04 max |
| S | 0.030 max |
| Cr | 15.0 - 17.5 |
| Ni | 3.0 - 5.0 |
| Cu | 3.0 - 5.0 |
| Nb+Ta | 0.15 - 0.45 |
| Condition | Tensile Strength (MPa) | Yield Strength 0.2% Proof (MPa) | Elongation (% in 50mm) | Hardness Rockwell C (HRC) | Hardness Brinell (HB) |
|---|---|---|---|---|---|
| Solution Treated | 1105 typ | 1000 typ | 15 typ | 38 max | 363 max |
| Condition 900 | 1310 min | 1170 min | 10 min | 40 min | 388 min |
| Condition 1150 | 930 min | 724 min | 16 min | 28 min | 277 min |
| Property | Value |
|---|---|
| Density (kg/m³) | 7750 |
| Mean Coefficient of Thermal Expansion 0-100°C (µm/m/°C) | 10.8 |
| Mean Coefficient of Thermal Expansion 0-315°C (µm/m/°C) | 11.6 |
| Thermal Conductivity at 100°C (W/m·K) | 18.4 |
| Thermal Conductivity at 500°C (W/m·K) | 22.7 |
| Specific Heat 0-100°C (J/kg·K) | 460 |
| Electrical Resistivity (nΩ·m) | 800 |
| Applications | Standards |
|---|---|
|
|
| Element | Content (%) |
|---|---|
| C | 0.07 max |
| Mn | 1.0 max |
| Si | 1.0 max |
| P | 0.04 max |
| S | 0.030 max |
| Cr | 15.0 - 17.5 |
| Ni | 3.0 - 5.0 |
| Cu | 3.0 - 5.0 |
| Nb+Ta | 0.15 - 0.45 |
| Condition | Tensile Strength (MPa) | Yield Strength 0.2% Proof (MPa) | Elongation (% in 50mm) | Hardness Rockwell C (HRC) | Hardness Brinell (HB) |
|---|---|---|---|---|---|
| Solution Treated | 1105 typ | 1000 typ | 15 typ | 38 max | 363 max |
| Condition 900 | 1310 min | 1170 min | 10 min | 40 min | 388 min |
| Condition 1150 | 930 min | 724 min | 16 min | 28 min | 277 min |
| Property | Value |
|---|---|
| Density (kg/m³) | 7750 |
| Mean Coefficient of Thermal Expansion 0-100°C (µm/m/°C) | 10.8 |
| Mean Coefficient of Thermal Expansion 0-315°C (µm/m/°C) | 11.6 |
| Thermal Conductivity at 100°C (W/m·K) | 18.4 |
| Thermal Conductivity at 500°C (W/m·K) | 22.7 |
| Specific Heat 0-100°C (J/kg·K) | 460 |
| Electrical Resistivity (nΩ·m) | 800 |