| Cuota De Producción: | 100 |
| Precio: | 3.65 |
| ASTM | JIS | AISI | EN |
|---|---|---|---|
| S30100 | SUS301 | 301 | 1.431 |
| S30400 | SUS304 | 304 | 1.4301 |
| S30403 | - | 304L | 1.4307 |
| S31008 | SUS310S | 310S | 1.4845 |
| S31603 | - | 316L | 1.4404 |
| S32100 | SUS321 | 321 | 1.4541 |
| S41008 | SUS410S | 410S | - |
| S43000 | SUS430 | 430 | 1.4016 |
| S43932 | - | - | 1.451 |
| S44400 | SUS444 | 444 | 1.4521 |
| S44500 | SUS430J1L | - | - |
| Element | Min (%) | Max (%) |
|---|---|---|
| C | 0.05 | 0.10 |
| Mn | - | 0.80 |
| Si | 1.10 | 2.00 |
| P | - | 0.040 |
| S | - | 0.030 |
| Cr | 20.0 | 22.0 |
| Ni | 10.0 | 12.0 |
| N | 0.14 | 0.20 |
| Ce | 0.03 | 0.08 |
| Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness Rockwell B (HR B) max | Hardness Brinell (HB) max |
|---|---|---|---|---|
| 600 | 310 | 40 | 95 | 217 |
| Property | Value |
|---|---|
| Density (kg/m³) | 7800 |
| Elastic Modulus (GPa) | 200 |
| Mean Coefficient of Thermal Expansion (mm/m/°C) 0-100°C | 17.0 |
| Mean Coefficient of Thermal Expansion (mm/m/°C) 0-600°C | 18.5 |
| Mean Coefficient of Thermal Expansion (mm/m/°C) 0-1000°C | 19.5 |
| Thermal Conductivity (W/m.K) at 20°C | 15.0 |
| Thermal Conductivity (W/m.K) at 1000°C | 29.0 |
| Specific Heat 0-100°C (J/kg.K) | 500 |
| Electrical Resistivity (nW.m) | 850 |
| UNS No | Old British BS | Euronorm No | Euronorm Name | Swedish SS | Japanese JIS |
|---|---|---|---|---|---|
| S30815 | - | 1.4835 | X9CrNiSiNCe21-11-2 | 2368 | - |
| Grade | Why it might be chosen instead of 253MA |
|---|---|
| 310 | Carburising atmospheres require a higher nickel content |
| 304H | Lower cost alternative, provided the operating temperature is below about 800°C |
| Nickel Alloys | Carburising atmospheres or temperatures above the 1100 - 1150°C maximum of 253MA |
| Cuota De Producción: | 100 |
| Precio: | 3.65 |
| ASTM | JIS | AISI | EN |
|---|---|---|---|
| S30100 | SUS301 | 301 | 1.431 |
| S30400 | SUS304 | 304 | 1.4301 |
| S30403 | - | 304L | 1.4307 |
| S31008 | SUS310S | 310S | 1.4845 |
| S31603 | - | 316L | 1.4404 |
| S32100 | SUS321 | 321 | 1.4541 |
| S41008 | SUS410S | 410S | - |
| S43000 | SUS430 | 430 | 1.4016 |
| S43932 | - | - | 1.451 |
| S44400 | SUS444 | 444 | 1.4521 |
| S44500 | SUS430J1L | - | - |
| Element | Min (%) | Max (%) |
|---|---|---|
| C | 0.05 | 0.10 |
| Mn | - | 0.80 |
| Si | 1.10 | 2.00 |
| P | - | 0.040 |
| S | - | 0.030 |
| Cr | 20.0 | 22.0 |
| Ni | 10.0 | 12.0 |
| N | 0.14 | 0.20 |
| Ce | 0.03 | 0.08 |
| Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness Rockwell B (HR B) max | Hardness Brinell (HB) max |
|---|---|---|---|---|
| 600 | 310 | 40 | 95 | 217 |
| Property | Value |
|---|---|
| Density (kg/m³) | 7800 |
| Elastic Modulus (GPa) | 200 |
| Mean Coefficient of Thermal Expansion (mm/m/°C) 0-100°C | 17.0 |
| Mean Coefficient of Thermal Expansion (mm/m/°C) 0-600°C | 18.5 |
| Mean Coefficient of Thermal Expansion (mm/m/°C) 0-1000°C | 19.5 |
| Thermal Conductivity (W/m.K) at 20°C | 15.0 |
| Thermal Conductivity (W/m.K) at 1000°C | 29.0 |
| Specific Heat 0-100°C (J/kg.K) | 500 |
| Electrical Resistivity (nW.m) | 850 |
| UNS No | Old British BS | Euronorm No | Euronorm Name | Swedish SS | Japanese JIS |
|---|---|---|---|---|---|
| S30815 | - | 1.4835 | X9CrNiSiNCe21-11-2 | 2368 | - |
| Grade | Why it might be chosen instead of 253MA |
|---|---|
| 310 | Carburising atmospheres require a higher nickel content |
| 304H | Lower cost alternative, provided the operating temperature is below about 800°C |
| Nickel Alloys | Carburising atmospheres or temperatures above the 1100 - 1150°C maximum of 253MA |