| MOQ: | 100 |
| preço: | 3.65 |
| ASTM | JIS | AISI | O que fazer? |
|---|---|---|---|
| S30100 | SUS301 | 301 | 1.431 |
| S30400 | SUS304 | 304 | 1.4301 |
| S30403 | - | 304L | 1.4307 |
| S31008 | SUS310S | 310S | 1.4845 |
| S31603 | - | 316L | 1.4404 |
| S32100 | SUS321 | 321 | 1.4541 |
| S41008 | SUS410S | 410S | - |
| S43000 | SUS430 | 430 | 1.4016 |
| S43932 | - | - | 1.451 |
| S44400 | SUS444 | 444 | 1.4521 |
| S44500 | SUS430J1L | - | - |
| ASTM A182 Grau FXM-19 | ASTM A269 Grau TPXM-19 | Classe ASTM A580 S20910 |
| ASTM A193 Grau B8R Classe 1C | ASTM A276 Grau S20910 | A classificação ASTM A813 TPXM-19 |
| ASTM A193, grau B8R classe 1D | A classificação ASTM A312 TPXM-19 | A classificação ASTM A814 TPXM-19 |
| Classe A193 ASTM B8RA Classe 1C | ASTM A314 Grau S20910 | ASTM A943 Grau TPXM-19 |
| ASTM A194 Grau 8R | ASTM A336 Grau FXM-19 | ASTM A959 Grau S20910 |
| ASTM A194 Grau 8RA | ASTM A358 Grau A240 XM-19 | Classe ASTM A965 FXM-19 |
| ASTM A213 Grau XM-19 | ASTM A403 Grau CRXM-19 | AISI XM-19 |
| ASTM A240 Grau S20910 | Classe ASTM A403 WPXM-19 | SAE XM-19 |
| ASTM A249 Grau TPXM-19 | ASTM A479 Grau S20910 | UNS S20910 |
| Elementos | Min (%) | Max (%) |
|---|---|---|
| C | 0.05 | 0.10 |
| - Não | - | 0.80 |
| Sim | 1.10 | 2.00 |
| P | - | 0.040 |
| S | - | 0.030 |
| Cr | 20.0 | 22.0 |
| Não. | 10.0 | 12.0 |
| N | 0.14 | 0.20 |
| C | 0.03 | 0.08 |
| Resistência à tração (MPa) min | Resistência ao rendimento 0,2% Proof (MPa) min | Elongação (% em 50 mm) min | Rockwell B (HR B) máximo | Brinell (HB) máximo |
|---|---|---|---|---|
| 600 | 310 | 40 | 95 | 217 |
| Densidade (kg/m3) | Modulo elástico (GPa) | Coeficiente médio de expansão térmica (mm/m/°C) | Conductividade térmica (W/m.K) | Calor específico 0-100°C (J/kg.K) | Resistividade elétrica (nW.m) | |||
|---|---|---|---|---|---|---|---|---|
| 0-100°C | 0-600°C | 0-1000°C | a 20°C | a 1000°C | ||||
| 7800 | 200 | 17.0 | 18.5 | 19.5 | 15.0 | 29.0 | 500 | 850 |
| Número da UNS | BS britânico | En britânico | Euronorm Não | Nome da Euronorm | SS sueco | JIS japonês |
|---|---|---|---|---|---|---|
| S30815 | - | - | 1.4835 | X9CrNiSiNCe21-11-2 | 2368 | - |
| Grau | Por que será escolhido em vez do 253MA? |
|---|---|
| 310 | As atmosferas de carburização exigem um teor de níquel mais elevado |
| 304H | Alternativa de menor custo, desde que a temperatura de funcionamento seja inferior a cerca de 800°C |
| Alcoóis de níquel | Atmosferas ou temperaturas de carburização superiores a 1100 - 1150 °C, máximo de 253 MA |
| MOQ: | 100 |
| preço: | 3.65 |
| ASTM | JIS | AISI | O que fazer? |
|---|---|---|---|
| S30100 | SUS301 | 301 | 1.431 |
| S30400 | SUS304 | 304 | 1.4301 |
| S30403 | - | 304L | 1.4307 |
| S31008 | SUS310S | 310S | 1.4845 |
| S31603 | - | 316L | 1.4404 |
| S32100 | SUS321 | 321 | 1.4541 |
| S41008 | SUS410S | 410S | - |
| S43000 | SUS430 | 430 | 1.4016 |
| S43932 | - | - | 1.451 |
| S44400 | SUS444 | 444 | 1.4521 |
| S44500 | SUS430J1L | - | - |
| ASTM A182 Grau FXM-19 | ASTM A269 Grau TPXM-19 | Classe ASTM A580 S20910 |
| ASTM A193 Grau B8R Classe 1C | ASTM A276 Grau S20910 | A classificação ASTM A813 TPXM-19 |
| ASTM A193, grau B8R classe 1D | A classificação ASTM A312 TPXM-19 | A classificação ASTM A814 TPXM-19 |
| Classe A193 ASTM B8RA Classe 1C | ASTM A314 Grau S20910 | ASTM A943 Grau TPXM-19 |
| ASTM A194 Grau 8R | ASTM A336 Grau FXM-19 | ASTM A959 Grau S20910 |
| ASTM A194 Grau 8RA | ASTM A358 Grau A240 XM-19 | Classe ASTM A965 FXM-19 |
| ASTM A213 Grau XM-19 | ASTM A403 Grau CRXM-19 | AISI XM-19 |
| ASTM A240 Grau S20910 | Classe ASTM A403 WPXM-19 | SAE XM-19 |
| ASTM A249 Grau TPXM-19 | ASTM A479 Grau S20910 | UNS S20910 |
| Elementos | Min (%) | Max (%) |
|---|---|---|
| C | 0.05 | 0.10 |
| - Não | - | 0.80 |
| Sim | 1.10 | 2.00 |
| P | - | 0.040 |
| S | - | 0.030 |
| Cr | 20.0 | 22.0 |
| Não. | 10.0 | 12.0 |
| N | 0.14 | 0.20 |
| C | 0.03 | 0.08 |
| Resistência à tração (MPa) min | Resistência ao rendimento 0,2% Proof (MPa) min | Elongação (% em 50 mm) min | Rockwell B (HR B) máximo | Brinell (HB) máximo |
|---|---|---|---|---|
| 600 | 310 | 40 | 95 | 217 |
| Densidade (kg/m3) | Modulo elástico (GPa) | Coeficiente médio de expansão térmica (mm/m/°C) | Conductividade térmica (W/m.K) | Calor específico 0-100°C (J/kg.K) | Resistividade elétrica (nW.m) | |||
|---|---|---|---|---|---|---|---|---|
| 0-100°C | 0-600°C | 0-1000°C | a 20°C | a 1000°C | ||||
| 7800 | 200 | 17.0 | 18.5 | 19.5 | 15.0 | 29.0 | 500 | 850 |
| Número da UNS | BS britânico | En britânico | Euronorm Não | Nome da Euronorm | SS sueco | JIS japonês |
|---|---|---|---|---|---|---|
| S30815 | - | - | 1.4835 | X9CrNiSiNCe21-11-2 | 2368 | - |
| Grau | Por que será escolhido em vez do 253MA? |
|---|---|
| 310 | As atmosferas de carburização exigem um teor de níquel mais elevado |
| 304H | Alternativa de menor custo, desde que a temperatura de funcionamento seja inferior a cerca de 800°C |
| Alcoóis de níquel | Atmosferas ou temperaturas de carburização superiores a 1100 - 1150 °C, máximo de 253 MA |