| MOQ: | 50 |
| τιμή: | 3.45 |
| Products | 17-4PH Stainless Steel Round Bar |
| Standard | ASTM GB DIN EN |
| Diameter | 8 - 450mm |
| Length | 6m /pcs or cutting as request |
| Finishing | black bar / Bright Bar |
| Main Grade | 201 301 303Cu 304 304L 309S 310S 316L 316Ti 317L 318 321 347 410 420 430 431 440a/b/c 904L 2205 2507 Hastelloy C276 C4 C22 Inconel 600 625 Incoloy 800 825 825H.etc |
| Service | Cutting, surface polishing, heat treatment |
| Brand | Walsin BAOSTEEL TISCO QINGSHAN |
| Applications | Standards |
|---|---|
|
|
| Grade | C | Mn | Si | P | S | Cr | Ni | Cu | Nb+Ta |
|---|---|---|---|---|---|---|---|---|---|
| 630 | min. max - 0.07 | - 1 | - 1 | - 0.04 | - 0.030 | 15 17.5 | 3 5 | 3 5 | 0.15 0.45 |
| Condition | Tensile Strength (MPa) | Yield Strength 0.2% Proof (MPa) | Elongation (% in 50mm) | Hardness Rockwell C (HR C) | Hardness Brinell (HB) |
|---|---|---|---|---|---|
| Solution Treated | 1105 typ | 1000 typ | 15 typ | 38 max | 363 max |
| Condition 900 | 1310 min | 1170 min | 10 min | 40 min | 388 min |
| Condition 1150 | 930 min | 724 min | 16 min | 28 min | 277 min |
| Mean Co-eff of Thermal Expansion (µm/m/°C) | Thermal Conductivity (W/m.K) | Specific Heat 0-100°C (J/kg.K) | Elec Resistivity (nΩ.m) |
|---|---|---|---|
| 0-100°C: 10.8 0-315°C: 11.6 0-538°C: - |
At 100°C: 18.4 At 500°C: 22.7 |
460 | 800 |
| MOQ: | 50 |
| τιμή: | 3.45 |
| Products | 17-4PH Stainless Steel Round Bar |
| Standard | ASTM GB DIN EN |
| Diameter | 8 - 450mm |
| Length | 6m /pcs or cutting as request |
| Finishing | black bar / Bright Bar |
| Main Grade | 201 301 303Cu 304 304L 309S 310S 316L 316Ti 317L 318 321 347 410 420 430 431 440a/b/c 904L 2205 2507 Hastelloy C276 C4 C22 Inconel 600 625 Incoloy 800 825 825H.etc |
| Service | Cutting, surface polishing, heat treatment |
| Brand | Walsin BAOSTEEL TISCO QINGSHAN |
| Applications | Standards |
|---|---|
|
|
| Grade | C | Mn | Si | P | S | Cr | Ni | Cu | Nb+Ta |
|---|---|---|---|---|---|---|---|---|---|
| 630 | min. max - 0.07 | - 1 | - 1 | - 0.04 | - 0.030 | 15 17.5 | 3 5 | 3 5 | 0.15 0.45 |
| Condition | Tensile Strength (MPa) | Yield Strength 0.2% Proof (MPa) | Elongation (% in 50mm) | Hardness Rockwell C (HR C) | Hardness Brinell (HB) |
|---|---|---|---|---|---|
| Solution Treated | 1105 typ | 1000 typ | 15 typ | 38 max | 363 max |
| Condition 900 | 1310 min | 1170 min | 10 min | 40 min | 388 min |
| Condition 1150 | 930 min | 724 min | 16 min | 28 min | 277 min |
| Mean Co-eff of Thermal Expansion (µm/m/°C) | Thermal Conductivity (W/m.K) | Specific Heat 0-100°C (J/kg.K) | Elec Resistivity (nΩ.m) |
|---|---|---|---|
| 0-100°C: 10.8 0-315°C: 11.6 0-538°C: - |
At 100°C: 18.4 At 500°C: 22.7 |
460 | 800 |