| Cuota De Producción: | 50 |
| Precio: | 3.44 |
| Product | 17-4PH Stainless Steel Round Bar |
|---|---|
| Standard | ASTM GB DIN EN |
| Diameter | 8 - 450mm |
| Length | 6m /pcs or cutting as requested |
| Finishing | Black Bar / Bright Bar |
| Main Grades | 201, 301, 303Cu, 304, 304L, 309S, 310S, 316L, 316Ti, 317L, 318, 321, 347, 410, 420, 430, 431, 440a/b/c, 904L, 2205, 2507, Hastelloy C276, C4, C22, Inconel 600, 625, Incoloy 800, 825, 825H, etc. |
| Service | Cutting, surface polishing, heat treatment |
| Brand | Walsin, BAOSTEEL, TISCO, QINGSHAN |
| Element | Content (%) |
|---|---|
| C | ≤ 0.07 |
| Mn | ≤ 1.00 |
| Si | ≤ 1.00 |
| P | ≤ 0.04 |
| S | ≤ 0.030 |
| Cr | 15.00 - 17.50 |
| Ni | 3.00 - 5.00 |
| Cu | 3.00 - 5.00 |
| Nb+Ta | 0.15 - 0.45 |
| Condition | Tensile Strength (MPa) | Yield Strength 0.2% Proof (MPa) | Elongation (% in 50mm) | Hardness Rockwell C (HRC) |
|---|---|---|---|---|
| Solution Treated | 1105 (typ) | 1000 (typ) | 15 (typ) | 38 max |
| Condition 900 | 1310 min | 1170 min | 10 min | 40 min |
| Condition 1150 | 930 min | 724 min | 16 min | 28 min |
| Property | Value |
|---|---|
| Density | 7750 kg/m³ |
| Thermal Conductivity (at 100°C) | 18.4 W/m·K |
| Thermal Conductivity (at 500°C) | 22.7 W/m·K |
| Specific Heat (0-100°C) | 460 J/kg·K |
| Electrical Resistivity | 800 nΩ·m |
| Mean Coefficient of Thermal Expansion (0-100°C) | 10.8 µm/m·°C |
| Mean Coefficient of Thermal Expansion (0-315°C) | 11.6 µm/m·°C |
| Alternative Grade | Reason for Choosing 17-4PH |
|---|---|
| 431 | 431 has higher toughness but 17-4PH offers better strength characteristics |
| 416 | 416 is free-machining but 17-4PH provides superior strength |
| 316 | 316 has higher corrosion resistance but much lower strength than 17-4PH |
| 2205 | 2205 offers better corrosion resistance with lower strength than 17-4PH |
| Condition | Hardening Temp (°C) | Time (h) | Typical Hardness (HRC) | Tensile Strength (MPa) |
|---|---|---|---|---|
| A | Ann | - | 36 | 1100 |
| H900 | 482 | 1 | 44 | - |
| H925 | 496 | 4 | 42 | 1170-1320 |
| H1025 | 552 | 4 | 38 | 1070-1220 |
| H1075 | 580 | 4 | 36 | 1000-1150 |
| H1100 | 593 | 4 | 35 | 970-1120 |
| H1150 | 621 | 4 | 33 | 930-1080 |
| Cuota De Producción: | 50 |
| Precio: | 3.44 |
| Product | 17-4PH Stainless Steel Round Bar |
|---|---|
| Standard | ASTM GB DIN EN |
| Diameter | 8 - 450mm |
| Length | 6m /pcs or cutting as requested |
| Finishing | Black Bar / Bright Bar |
| Main Grades | 201, 301, 303Cu, 304, 304L, 309S, 310S, 316L, 316Ti, 317L, 318, 321, 347, 410, 420, 430, 431, 440a/b/c, 904L, 2205, 2507, Hastelloy C276, C4, C22, Inconel 600, 625, Incoloy 800, 825, 825H, etc. |
| Service | Cutting, surface polishing, heat treatment |
| Brand | Walsin, BAOSTEEL, TISCO, QINGSHAN |
| Element | Content (%) |
|---|---|
| C | ≤ 0.07 |
| Mn | ≤ 1.00 |
| Si | ≤ 1.00 |
| P | ≤ 0.04 |
| S | ≤ 0.030 |
| Cr | 15.00 - 17.50 |
| Ni | 3.00 - 5.00 |
| Cu | 3.00 - 5.00 |
| Nb+Ta | 0.15 - 0.45 |
| Condition | Tensile Strength (MPa) | Yield Strength 0.2% Proof (MPa) | Elongation (% in 50mm) | Hardness Rockwell C (HRC) |
|---|---|---|---|---|
| Solution Treated | 1105 (typ) | 1000 (typ) | 15 (typ) | 38 max |
| Condition 900 | 1310 min | 1170 min | 10 min | 40 min |
| Condition 1150 | 930 min | 724 min | 16 min | 28 min |
| Property | Value |
|---|---|
| Density | 7750 kg/m³ |
| Thermal Conductivity (at 100°C) | 18.4 W/m·K |
| Thermal Conductivity (at 500°C) | 22.7 W/m·K |
| Specific Heat (0-100°C) | 460 J/kg·K |
| Electrical Resistivity | 800 nΩ·m |
| Mean Coefficient of Thermal Expansion (0-100°C) | 10.8 µm/m·°C |
| Mean Coefficient of Thermal Expansion (0-315°C) | 11.6 µm/m·°C |
| Alternative Grade | Reason for Choosing 17-4PH |
|---|---|
| 431 | 431 has higher toughness but 17-4PH offers better strength characteristics |
| 416 | 416 is free-machining but 17-4PH provides superior strength |
| 316 | 316 has higher corrosion resistance but much lower strength than 17-4PH |
| 2205 | 2205 offers better corrosion resistance with lower strength than 17-4PH |
| Condition | Hardening Temp (°C) | Time (h) | Typical Hardness (HRC) | Tensile Strength (MPa) |
|---|---|---|---|---|
| A | Ann | - | 36 | 1100 |
| H900 | 482 | 1 | 44 | - |
| H925 | 496 | 4 | 42 | 1170-1320 |
| H1025 | 552 | 4 | 38 | 1070-1220 |
| H1075 | 580 | 4 | 36 | 1000-1150 |
| H1100 | 593 | 4 | 35 | 970-1120 |
| H1150 | 621 | 4 | 33 | 930-1080 |