| Cuota De Producción: | 50 |
| Precio: | 2.58 |
| Applications | Standards |
|---|---|
|
|
| Element | Content (%) |
|---|---|
| C | 0.07 max |
| Mn | 1.0 max |
| Si | 1.0 max |
| P | 0.04 max |
| S | 0.030 max |
| Cr | 15.0 - 17.5 |
| Ni | 3.0 - 5.0 |
| Cu | 3.0 - 5.0 |
| Nb+Ta | 0.15 - 0.45 |
| Condition | Tensile Strength (MPa) | Yield Strength 0.2% Proof (MPa) | Elongation (% in 50mm) | Hardness Rockwell C (HRC) |
|---|---|---|---|---|
| Solution Treated | 1105 typ | 1000 typ | 15 typ | 38 max |
| Condition 900 | 1310 min | 1170 min | 10 min | 40 min |
| Condition 1150 | 930 min | 724 min | 16 min | 28 min |
| Property | Value |
|---|---|
| Density (kg/m³) | 7750 |
| Thermal Conductivity at 100°C (W/m·K) | 18.4 |
| Thermal Conductivity at 500°C (W/m·K) | 22.7 |
| Specific Heat 0-100°C (J/kg·K) | 460 |
| Electrical Resistivity (nΩ·m) | 800 |
| Condition | Hardening Temp (°C) | Time (h) | Typical Hardness Rockwell C | Tensile Strength (MPa) |
|---|---|---|---|---|
| A | Ann | - | 36 | 1100 |
| H900 | 482 | 1 | 44 | - |
| H925 | 496 | 4 | 42 | 1170-1320 |
| H1025 | 552 | 4 | 38 | 1070-1220 |
| H1075 | 580 | 4 | 36 | 1000-1150 |
| H1100 | 593 | 4 | 35 | 970-1120 |
| H1150 | 621 | 4 | 33 | 930-1080 |
| Cuota De Producción: | 50 |
| Precio: | 2.58 |
| Applications | Standards |
|---|---|
|
|
| Element | Content (%) |
|---|---|
| C | 0.07 max |
| Mn | 1.0 max |
| Si | 1.0 max |
| P | 0.04 max |
| S | 0.030 max |
| Cr | 15.0 - 17.5 |
| Ni | 3.0 - 5.0 |
| Cu | 3.0 - 5.0 |
| Nb+Ta | 0.15 - 0.45 |
| Condition | Tensile Strength (MPa) | Yield Strength 0.2% Proof (MPa) | Elongation (% in 50mm) | Hardness Rockwell C (HRC) |
|---|---|---|---|---|
| Solution Treated | 1105 typ | 1000 typ | 15 typ | 38 max |
| Condition 900 | 1310 min | 1170 min | 10 min | 40 min |
| Condition 1150 | 930 min | 724 min | 16 min | 28 min |
| Property | Value |
|---|---|
| Density (kg/m³) | 7750 |
| Thermal Conductivity at 100°C (W/m·K) | 18.4 |
| Thermal Conductivity at 500°C (W/m·K) | 22.7 |
| Specific Heat 0-100°C (J/kg·K) | 460 |
| Electrical Resistivity (nΩ·m) | 800 |
| Condition | Hardening Temp (°C) | Time (h) | Typical Hardness Rockwell C | Tensile Strength (MPa) |
|---|---|---|---|---|
| A | Ann | - | 36 | 1100 |
| H900 | 482 | 1 | 44 | - |
| H925 | 496 | 4 | 42 | 1170-1320 |
| H1025 | 552 | 4 | 38 | 1070-1220 |
| H1075 | 580 | 4 | 36 | 1000-1150 |
| H1100 | 593 | 4 | 35 | 970-1120 |
| H1150 | 621 | 4 | 33 | 930-1080 |